An aggregate which passes through 25 mm IS sieve and is retained on at 20 mm IS sieve, is said to be flaky if its least dimension is less than ______

A
22.5 mm
No worries! We‘ve got your back. Try BYJU‘S free classes today!
B
18.5 mm
No worries! We‘ve got your back. Try BYJU‘S free classes today!
C
16.5 mm
No worries! We‘ve got your back. Try BYJU‘S free classes today!
D
13.5 mm
Right on! Give the BNAT exam to get a 100% scholarship for BYJUS courses
Open in App
Solution

The correct option is D 13.5 mm
The aggregates are said to be flaky if their least dimension is less than 0.6 times their average dimension.
If the aggregate passes through a 25 mm sieve and is retained on a 20 mm sieve, then their mean dimension equals
20+252 = 22.5 mm

So, as per definition of flaky aggregate the aggregate is said to be flaky if its least dimension is less than
0.6×22.5 = 13.5 mm.

flag
Suggest Corrections
thumbs-up
0
Join BYJU'S Learning Program
similar_icon
Related Videos
thumbnail
lock
Flakiness Index
OTHER
Watch in App
Join BYJU'S Learning Program
CrossIcon