IS : 1343-1980 limits the minimum characteristic strength of pre-stressed concrete for post-tensioned work and pre-tensioned work as
A
25 MPa, 30 MPa respectively
No worries! Weāve got your back. Try BYJUāS free classes today!
B
25 MPa, 35 MPa respectively
No worries! Weāve got your back. Try BYJUāS free classes today!
C
30 MPa, 35 MPa respectively
No worries! Weāve got your back. Try BYJUāS free classes today!
D
30 MPa, 40 MPa respectively
Right on! Give the BNAT exam to get a 100% scholarship for BYJUS courses
Open in App
Solution
The correct option is D 30 MPa, 40 MPa respectively Minimum characteristic strength of prestressed concrete for
Post tensioned = 30 MPa
Pre tensioned = 40 MPa