Match List-I (welding defects) with List-II (Causes) and select the correct answer using the codes given below the lists:

Lis-I List-II
A. Spatter 1. Damp electrodes
B. Distortion 2. Arc blow
C. Slag inclusion 3. Improper cleaning in multi pass welding
D. Porosity 4. Poor joint selection

Codes
ABCD​​​

A
2413
No worries! We‘ve got your back. Try BYJU‘S free classes today!
B
2431
Right on! Give the BNAT exam to get a 100% scholarship for BYJUS courses
C
4213
No worries! We‘ve got your back. Try BYJU‘S free classes today!
D
4231
No worries! We‘ve got your back. Try BYJU‘S free classes today!
Open in App
Solution

The correct option is B 2431
2431

flag
Suggest Corrections
thumbs-up
1
Join BYJU'S Learning Program
similar_icon
Related Videos
thumbnail
lock
Appearance
CHEMISTRY
Watch in App
Join BYJU'S Learning Program
CrossIcon