Products obtained during catalytic oxidation of ammonia are?
A mixture of dry air and dry ammonia in the ratio of 10:1 by volume is compressed and then
passed into a platinum gauze which acts as catalyst at about 800°C.Below is the reaction for the same.
4NH3+5O2800oC−−−−−→Pt.guage4NO+6H2O+Heat