The amount of tetracalcium aluminoferrite that is responsible for flash set but generates less heat is required approximately ______ of cement.
A
16 - 20 %
No worries! We‘ve got your back. Try BYJU‘S free classes today!
B
8 - 14 %
Right on! Give the BNAT exam to get a 100% scholarship for BYJUS courses
C
25 - 40 %
No worries! We‘ve got your back. Try BYJU‘S free classes today!
D
5 - 7 %
No worries! We‘ve got your back. Try BYJU‘S free classes today!
Open in App
Solution
The correct option is B 8 - 14 % The amount of tetracalcium aluminoferrite that is responsible for flash set but generates less heat required is approximately 8 - 14% of cement. It has the poorest cementing value, raising the C4AF content reduces the strength slightly.