The correct options are
A Platinum
B Vanadium pentoxide
The second stage of the contact process involves oxidation of Sulphur dioxide(SO2) to Sulphur trioxide(SO3). Since this is a very slow process, the gases are passed through granulated catalyst such as platinum or vanadium pentoxide at a temperature of 450oC.